We watch the cavity fill before any steel is cut
Mold flow analysis is a simulation of how molten plastic fills, packs and cools inside a mold. We feed the software with the 3D part model, the selected resin and the intended process conditions; it returns fill time, pressure and temperature distribution, the position of weld lines and air traps, and the tendency of the part to sink or warp.
At OSKA we run this analysis in-house. The people who read the results, design the mold and machine the steel work in the same workshop, so a problem seen on screen goes straight back into the design. The goal is simple: find the fault before chips are cut, not at the mold trial.
Questions the analysis answers
- Does the part fill evenly, or is there a risk of short shots and hesitation?
- How many gates are needed, where should they sit and how large should they be?
- Where do weld lines form, and do they fall on a visible or load-bearing area?
- Where does air get trapped, and where should vents be placed?
- Which areas are prone to sink marks, burn marks or discoloration?
- How much will the part warp and in which direction? Will flatness tolerances hold?
- Is the cooling layout sufficient, or are there hot spots in the mold?
- What clamp force is required, and which machine size suits the part?
When we use it
1. While the part is still being designed
Fill, shrinkage and warpage results show where ribs are needed, where wall thickness should be reduced or where the shape should change. At this stage a change is only a model update.
2. Before mold design starts
We run alternative gate positions, runner layouts and cooling options side by side and pick the most balanced one, so the design moves forward on compared data rather than guesswork.
3. When the mold design is complete
The finished design is checked once more as a whole for filling, packing, surface quality, shrinkage and cooling. Any correction is made before steel is ordered.
4. When a mold trial reveals a problem
We model the existing mold with the actual process settings to find a root cause that experience alone may miss. The proposed fix is verified in simulation first and only then applied to the mold, which reduces the number of trials and revisions.
How the work proceeds
- Define the goal: foreseeing risks in a new mold, or solving an issue such as short shots or warpage in a running one.
- Collect the data: 3D part model, mold layout, flow and thermal properties of the resin, and the intended process values.
- Build the mesh: the model is divided into small elements. Because accuracy depends on mesh quality, no free edges, intersecting or overlapping elements are left.
- Solve the filling, packing, cooling and warpage stages.
- Interpret the results: findings are reported to you together with the recommended design changes.
Main results we review
| Result | What we look at | Design decision it drives |
|---|---|---|
| Filling | Flow balance, fill time, unfilled areas | Gate position and count, wall thickness |
| Pressure distribution | Balanced, symmetric pressure in the cavity | Runner sizes, packing profile |
| Flow front temperature | Temperature drop or rise during filling | Injection speed, gate size |
| Clamp force | Tonnage needed to keep the mold closed | Machine selection, flash risk |
| Shear rate and shear stress | Whether resin limits are exceeded | Gate cross-section, fill speed |
| Weld lines | Position, visibility and effect on strength | Gate location, flow leaders |
| Air traps | Points where air is enclosed | Vent positions |
| Shrinkage and sink marks | Surface sinks in thick sections, dimensional deviation | Wall thickness, rib ratio, packing |
| Frozen layer | How much of the section has solidified, and when | Packing time, gate freeze time |
| Cooling | Temperature differences on the mold surface, hot spots | Cooling channel layout, cycle time |
| Warpage | Shape deviation after ejection | Geometry, gate location, cooling balance |
What you gain
- Design faults are caught before steel is machined, so less welding and rework on the mold.
- Fewer mold trials and a shorter path to series production.
- Balanced filling and correct cooling reduce scrap and cycle time.
- Decisions on gating, cooling and machine tonnage rest on data, reducing uncertainty at the quotation stage.
Parts for which we especially recommend it
- Thin-walled parts, long flow lengths or varying wall thickness
- Housings and covers with visible surfaces where weld lines and sink marks are not acceptable
- Multi-cavity molds where balanced filling matters
- Glass-fibre reinforced parts that are prone to warpage
- Functional parts with tight flatness and dimensional tolerances, such as fan impellers, lighting housings and snap-fit components
Flow analysis is a predictive tool. Real results vary with the resin lot, the machine and the process settings, so the analysis does not replace the mold trial; it makes sure we enter the trial prepared.
Frequently Asked Questions
Does every mold need a flow analysis?
No. For simple geometries similar to parts we have already made, experience is usually enough. The more complex the part and the stricter the surface and tolerance requirements, the more the analysis pays for itself.
What do you need from us?
The 3D model of the part (STEP or IGES), the resin type and, if possible, its trade name, plus the visible surfaces and critical dimensions. If the molding machine is known, please add that as well.
Is flow analysis the same as a DFM review?
No. DFM is a broader review of whether the part suits production in general. Flow analysis numerically models only the injection process: filling, packing and cooling. The two complement each other.
Can you analyse a mold that is already running?
Yes. For recurring problems such as short shots, warpage or burn marks we model the existing mold and process settings, look for the root cause and test the revision in simulation first.