When an aluminium part is to be CNC machined, the most frequent question is which alloy to use. The two most common options are 6061 (with 6082 as its close European counterpart) and 7075. Both machine well, but they do not give the same result.
Quick comparison
| Property | 6061 / 6082 (T6) | 7075 (T6) |
|---|---|---|
| Main alloying elements | Magnesium and silicon | Zinc |
| Tensile strength (approx.) | ~310 MPa | ~540–570 MPa |
| Hardness | Medium | Markedly higher |
| Weldability | Good | Poor; welding not advised |
| Corrosion resistance | Good | Lower; needs protection |
| Anodising | Even, decorative result | Possible; colour may be less uniform |
| Cost | More economical, widely available | More expensive |
When 6061 / 6082 is the right choice
- General-purpose parts: brackets, housings, covers, fixtures, guards.
- Parts that will be welded.
- Outdoor or humid service.
- Visible surfaces needing even, coloured anodising.
- When cost matters and loads are not at the limit.
When 7075 is the right choice
- Highly loaded parts where weight is critical.
- Thin sections that must resist bending and bearing loads.
- Threads and seating faces that must last without deforming.
- Short-run prototype molds or mold inserts.
Machining differences
Both alloys cut comfortably at high speeds. 7075 is harder, so its chips break short and the surface comes out clean; 6061 is softer and tends to build up on the tool without suitable tooling and coolant. On parts hollowed out of large plates, internal stresses can cause distortion; using stress-relieved plate and letting the part rest between roughing and finishing improves dimensional stability.