A drawing that only says “stainless” gives the machinist incomplete information. Stainless steels are a wide family whose machinability, corrosion resistance, hardenability and price differ greatly. Choosing the right grade determines both the life of the part and the cost of machining it.
Commonly used grades
| Grade (AISI / EN) | Structure | Key property | Machinability | Typical use |
|---|---|---|---|---|
| 303 / 1.4305 | Austenitic | Sulphur added; the easiest stainless to machine | Very good | Turned parts, shafts, fittings, fasteners |
| 304 / 1.4301 | Austenitic | General purpose; good corrosion resistance, weldable | Medium | Food equipment, housings, brackets |
| 316 / 1.4401 – 1.4404 | Austenitic | Molybdenum added; superior against chlorides and acids | Medium–difficult | Marine, chemical and medical parts |
| 430 / 1.4016 | Ferritic | Economical, magnetic | Good | Decorative parts, housewares |
| 420 / 1.4021 – 1.4028 | Martensitic | Hardens by heat treatment | Good (annealed) | Cutting and wear parts, shafts; mold steel variants for plastic mold cavities |
| 17-4 PH / 1.4542 | Precipitation hardening | High strength together with corrosion resistance | Medium | Highly loaded shafts, valve parts, aerospace |
| Duplex 2205 / 1.4462 | Austenitic-ferritic | High strength, resists stress corrosion | Difficult | Oil and gas, seawater equipment |
Three questions when choosing
- What is the environment? For indoor use and clean water 304 is usually enough. With salt, chlorine or acids, move up to 316.
- Does the part need to be hard? Austenitic grades (303, 304, 316) do not harden by heat treatment. For wear or cutting edges choose 420 or 17-4 PH.
- Is there welding or plating? Because of its sulphur, 303 is not suited to welding and resists corrosion less well than 304; for welded parts 304L or 316L is preferred.
On parts with heavy stock removal, no welding and no severely corrosive service, choosing 303 instead of 304 noticeably cuts machining time and tool consumption.
Why is stainless hard to machine?
- Work hardening: austenitic stainless hardens at the surface as it is cut. If the tool rubs, the next pass meets a much harder layer.
- Low thermal conductivity: heat does not leave with the chip; it builds up at the cutting edge and shortens tool life.
- Galling: material sticks to the cutting edge, forms a built-up edge and spoils the surface.
- Long, ductile chips: chips do not break and wrap around tool and part.
How we deal with it in the shop
- We use sharp, positive-geometry tools with suitable coatings and change worn tools immediately.
- We never let the tool dwell: feed is kept constant and sufficient, and light rubbing passes are avoided.
- Plenty of well-directed coolant takes heat away from the cutting zone.
- Part and tool are clamped rigidly; vibration increases work hardening.
- Deep holes and threads are cleared of chips in steps.
After machining
Free iron picked up during machining can later appear as rust stains on a stainless part. Passivation removes that iron and renews the protective oxide layer. For appearance, blasting, brushing (satin) or electropolishing can be applied. See our Surface Finishes Guide.
When asking for a quote
State the grade clearly on the drawing (for example 1.4301 or AISI 304) and add hardness and surface requirements if any. If you are unsure of the grade, describe where the part will work and we will settle the grade together.