Combining metal with plastic, or hard with soft plastic, in a single body removes assembly steps and gives a part new functions. There are three common ways to do it: insert molding, overmolding and two-shot (2K) molding.
Insert molding
A pre-made component — usually a brass threaded bush, a shaft, a contact or a sheet metal part — is placed in the mold and plastic is injected around it. The result is one part that combines the strength of metal with the design freedom of plastic.
- The insert needs knurls, grooves or holes on its outside; plastic fills them and prevents rotation and pull-out.
- The plastic wall around the insert must be thick enough; if it is too thin, hoop stress during cooling cracks it.
- The insert is held in the mold by a pin, pocket or magnet and must not move under injection pressure.
- Preheating large metal inserts reduces instant freezing of the melt on the metal and lowers internal stress.
- Insert tolerances must be tight: a loose insert flashes, a tight one damages the mold.
Overmolding
A rigid substrate is molded first, then placed in a second mold where a second material — usually a soft TPE or TPU — is molded over it. Grip surfaces, seals, bumpers and two-colour parts are made this way.
- The two materials must be chemically compatible. Without compatibility there is no bond, and a mechanical interlock (holes, grooves, wrap-around) has to be designed.
- A soft layer that is too thin freezes before it fills; 1.5–3 mm is generally a safe range.
- The edge where the soft material ends should be bounded by a step or groove in the substrate, otherwise it peels and flashes.
- The substrate must seat perfectly in the second mold; soft material leaks into every gap.
| Substrate | Bonding with TPE/TPU |
|---|---|
| ABS, PC, ABS/PC | Good (with a suitable TPE grade) |
| PP | Good (with PP-based TPE) |
| PA | Needs a special bonding grade |
| POM, PE | Poor; mechanical interlock recommended |
This is a general assessment; for a firm answer the resin supplier’s adhesion chart applies.
Two-shot (2K) molding
Two materials are injected one after the other on a single machine with two injection units, in one rotating or sliding mold. Because the second material is added before the part leaves the mold, bonding is better, there is no positioning error and the cycle is short. The trade-off is a high investment in mold and machine.
Which one, when?
| Method | Tool investment | Suitable volume | Note |
|---|---|---|---|
| Insert molding | Low–medium | Any | Inserts are loaded by hand or automatically |
| Overmolding (two molds) | Medium | Low–medium | Runs on standard machines, more labour |
| Two-shot (2K) | High | High | Best bond and shortest cycle |
Ask us before you start the design
The material pair, the boundary of the soft layer and the way the insert is held define the mold from the start. Share your model early and we will choose the most suitable method together.