Ana Sayfa / Casting Molds / Aluminium Die Casting Molds

Aluminium Die Casting Molds

Design and manufacture of aluminium high pressure die casting molds, die steel and common casting defects.

Türkçe

OverviewAdvantagesMold structureSteel and lifeDesign rulesDefects and fixesFAQ

Aluminium die casting (HPDC) molds

In aluminium die casting, molten aluminium is forced from the machine’s shot sleeve into the die cavity at high pressure and speed and solidifies within seconds. The process produces thin-walled, accurate, complex parts in high volumes. Motor and electronics housings, LED luminaire housings, heat sinks, brackets and covers are typical applications.

Part quality in this process is driven mainly by the die: runner and gate section, overflows, air and vacuum venting, thermal balance and core layout. At OSKA we design and machine aluminium die casting molds and deliver them ready for your foundry’s machine.

Advantages of aluminium die casting

  • Thin walls and complex shapes: high-pressure filling reaches thin, deep areas that other processes cannot cast.
  • Dimensional accuracy: many faces can be used as cast or with very little machining.
  • High productivity: cycle times are measured in seconds; the fastest casting process for series production.
  • Material use: near-net-shape casting reduces chips and scrap.
  • Light weight and heat conduction: aluminium is light, corrosion resistant and conducts heat well; ideal for heat sinks and housings.
  • EMI shielding: a metal housing protects electronics against interference.
  • Recycling: aluminium can be remelted and reused without losing its properties.

Parts of an aluminium die casting mold

Part Function
Fixed and moving half The two main bodies that form the outer and inner shape and are mounted on the machine platens
Cavity and core inserts Replaceable hot-work steel parts in contact with the molten metal
Shot sleeve and sprue bush Where the metal enters the die from the machine
Runners and gates Channels that distribute metal to the cavities evenly and at the right speed
Overflows Collect the first cold, oxidised metal and keep the far ends of the cavity filling hot
Air and vacuum venting Remove air from the cavity and reduce gas porosity
Slides and cores Form holes and recesses perpendicular to the opening direction
Cooling / heating channels Keep the die at the required temperature with water or oil; thermal balance drives dimensions and life
Ejector system Pushes the solidified casting out of the die

Die steel and life

A die casting die meets metal at around 650–700 °C with every shot and is then cooled. Over time this thermal cycle causes heat checking on the surface. Cavities and cores are therefore made from hot-work tool steels such as 1.2343 and 1.2344 (H11 / H13), hardened and nitrided where needed.

  • Preheating the die before the first shot prevents thermal shock and early cracking.
  • Regular stress relieving and surface maintenance extend die life.
  • Gates and cores that wear are designed as replaceable inserts, so the whole die does not have to be renewed.

Part design guidelines

  • Keep wall thickness as uniform as possible; thick sections cause shrinkage porosity.
  • Avoid sharp corners; inside radii also protect the die against cracking.
  • Give enough draft; castings shrink onto cores and stick or scratch without it.
  • Core out thick areas and stiffen them with ribs.
  • Leave machining allowance only where needed; machining can open up subsurface porosity.
  • For anodized parts agree the alloy early; high-silicon alloys give a dark, blotchy colour.

Common casting defects and their fixes

Defect Likely causes Fix in die and process
Misrun, unclear edges Low metal temperature, small gate, poor venting Larger gate, add overflows and vents, adjust metal and die temperature
Cold shut Two flow fronts meet after cooling Change runner layout, overflow at the meeting point, raise die temperature
Gas porosity and blisters Trapped air, too much release agent, wet metal Vacuum or better venting, less release agent, clean dry metal
Shrinkage porosity and sink Thick section, insufficient feeding Reduce wall thickness, local cooling, adjust intensification pressure
Cracks and hot tears Sharp corners, early ejection, uneven cooling Add radii, balance cooling, relocate ejectors
Soldering Overheated die surface, insufficient draft Local cooling, nitriding or PVD coating, more draft
Flash Worn die faces, insufficient clamping force Renew parting faces, choose the machine by projected area
Streaks after anodizing High silicon content, flow lines Suitable alloy, improved fill speed and gate layout

Frequently Asked Questions

Which machine sizes do you build dies for?

We design the die for your foundry’s machine. Share the clamping force, platen and tie-bar dimensions and shot sleeve diameter at the quotation stage.

Can die castings be heat treated?

In conventional die casting, trapped gas blisters at high temperature, so heat treatments such as T6 are generally not applied. If heat treatment is needed, vacuum die casting, gravity die or low pressure casting are considered.

Do you machine the castings?

Yes. We do post-casting CNC machining, drilling and tapping in our workshop.

Request a Quote

Kalıp ve hassas parça işleriniz için üretim ortağınız

Kokil, plastik enjeksiyon ve alüminyum enjeksiyon kalıpları ile CNC talaşlı imalat tek atölyede. Teknik resminizi gönderin, birlikte değerlendirelim.

Bize Ulaşın
Kasım 16, 2026

Stainless Steel Grades in CNC Machining: 303, 304, 316, 420 and 17-4 PH

Devamını oku
Kasım 16, 2026

CNC İşlemede Paslanmaz Çelik Türleri: 303, 304, 316, 420 ve 17-4 PH

Devamını oku
Tüm haberler ve yazılar