What is it?How it worksPros and limitsApplicationsMold designFAQ
Low pressure die casting molds
In low pressure die casting the mold sits on top of a sealed furnace holding molten metal. Dry air or nitrogen at low pressure pushes the metal up a riser tube and fills the cavity calmly from below. Pressure is held until the casting has fully solidified, then released, and the metal left in the tube falls back into the furnace.
This calm, controlled filling reduces oxide and gas entrapment and produces dense, sound castings. At OSKA we design and build molds for low pressure casting and deliver them ready for your foundry’s machine.
The casting cycle step by step
-
Mold closes
Die halves and any sand cores are set and the mold closes over the furnace.
-
Pressure rises
Pressure is applied to the furnace in a controlled way; metal rises up the tube towards the mold.
-
Filling
Metal enters the cavity from below and fills it calmly; air escapes from the upper areas.
-
Solidification under pressure
With pressure held, the casting solidifies from the far end towards the gate, which acts as the feeder.
-
Pressure released
Unsolidified metal returns to the furnace; no separate feeder is needed.
-
Mold opens
The casting is removed and the mold is prepared for the next cycle.
Advantages and limits
| Advantage | Limit |
|---|---|
| Calm bottom filling; less oxide and gas porosity | Cycle time is longer than die casting (a few minutes) |
| Dense structure; suits pressure-tight parts | Not suited to very thin walls; typical minimum about 3 mm |
| Heat treatment (T6) possible; high mechanical strength | Machine and mold investment higher than gravity die |
| Sand cores possible; complex internal passages | Dimensional accuracy lower than high pressure die casting |
| High metal yield, as no feeders are needed | Thermal management of the mold must be well designed |
Where it is used
- Automotive: wheels, cylinder heads, engine and transmission housings, intake manifolds.
- Machinery: hydraulic and water pump housings, oil pumps, fan blades, gearbox housings.
- Marine: propellers and housing parts.
- General industry: pressure-bearing, heat-treated aluminium housings, covers and discs.
Key points in low pressure mold design
- Directional solidification: the casting should solidify from the point furthest from the gate towards the gate, achieved by placing heavy sections near the gate and zoning mold temperature.
- Zoned cooling: air or water cooling zones set solidification order and cycle time; temperatures are monitored with thermocouples.
- Gate and filter: the gate seats on the riser tube; a ceramic filter keeps oxides out of the cavity.
- Venting: as filling runs bottom to top, vents and vent plugs are placed at the highest points of the cavity.
- Cores: steel or sand cores for internal passages; secure seating and gas escape of sand cores are designed in.
- Die coating: an insulating coating prevents premature freezing and helps release.
- Mold steel: hot-work tool steels for cavities and cores; wearing parts are designed as replaceable inserts.
Frequently Asked Questions
Low pressure or gravity die?
Both give sound, heat-treatable castings. For high volume, high metal yield and pressure tightness choose low pressure; for low to medium volume and lower investment, gravity die.
Low pressure or high pressure die casting?
Thin-walled, accurate, very high-volume parts suit high pressure die casting; thicker parts that need heat treatment and pressure tightness suit low pressure casting.
What should I send for a quote?
3D model, alloy, heat treatment requirement, annual volume and your casting machine mounting data.