OverviewHow it worksWhere we use itStrengths and limitsSinker vs wire EDMFAQ
Where the cutter cannot reach, the spark can
Sinker EDM (electrical discharge machining) removes material from electrically conductive workpieces with controlled sparks. There is no contact and no cutting force between tool and part, so sharp internal corners, deep narrow rib slots, fine grooves and complex forms can be produced even in hardened steel.
At OSKA sinker EDM is in-house. We machine the electrode on our vertical machining centre and erode the mold under the same roof. The mold does not leave the workshop for a single operation, and responsibility for the dimensions stays in one place.
How sinker EDM works
The reverse of the required form is prepared as an electrode in copper or graphite. Electrode and workpiece are brought very close together in a dielectric fluid without touching. Thousands of sparks per second jump across the small gap; each one melts and removes a microscopic particle of steel, and the fluid flushes the particles away. As the electrode advances step by step, its form is reproduced in the steel.
- Electrode design: the area to be eroded is separated from the 3D model and the electrode is modelled smaller by the spark gap.
- Electrode manufacture: roughing and finishing electrodes are milled on the machining centre.
- Set-up and alignment: electrode and mold part are positioned to the same reference.
- Rough erosion: most of the material is removed at high energy.
- Finish erosion: size and surface are brought to final values at low energy.
- Inspection: depth and form are measured; the surface is prepared for polishing if needed.
Where we use it in a mold
| Feature | Why EDM? |
|---|---|
| Deep, thin rib slots | A slender end mill deflects and breaks; an electrode reaches the same depth easily. |
| Sharp internal corners | A round cutter leaves a radius; an electrode gives the corner the sharpness required. |
| Hardened mold parts | Distortion from heat treatment is removed by eroding the final size afterwards. |
| Narrow deep pockets and fine grooves | Areas with no tool access or poor chip evacuation. |
| Lettering, logos and date stamps | Small raised or engraved details transfer cleanly from the electrode. |
| Matt (EDM) surface texture | The even matt texture left by the sparks gives the molded part a blasted-like appearance. |
Strengths and limits
Strengths
Limits
Sinker EDM and wire EDM
Both work with sparks but do different jobs. In sinker EDM a shaped electrode plunges into the part and produces blind cavities. In wire EDM a thin wire cuts right through the part from one side to the other, so it only suits through profiles.
| Sinker EDM | Wire EDM | |
|---|---|---|
| Tool | Shaped copper or graphite electrode | Continuously fed thin wire |
| Form produced | Blind cavities, rib slots, 3D forms | Through profiles, punch and die openings |
| Typical mold work | Cavity details, sharp corners, lettering | Insert pockets, ejector and core-pin profiles, cutting dies |
| At OSKA | In-house | Not available in-house |
Frequently Asked Questions
Do you accept EDM-only work?
Yes. We consider erosion jobs independently of a mold project, with the electrode made by us or supplied by you.
Copper or graphite electrode?
Copper excels at fine surfaces and sharp detail; graphite at large, deep forms with fast removal and low electrode wear. We choose according to the size of the form and the surface required.
What does an EDM surface look like on the part?
The spark texture transfers to the part as an even matt surface. For a glossy part the cavity is polished after erosion.
What do you need from us?
The 3D model, the areas to be eroded, the material and hardness, and the surface quality required.