Sinker EDM

Sharp corners, deep rib slots and fine detail in hardened steel, with electrode manufacture in our own workshop.

Türkçe sürüm

OverviewHow it worksWhere we use itStrengths and limitsSinker vs wire EDMFAQ

Where the cutter cannot reach, the spark can

Sinker EDM (electrical discharge machining) removes material from electrically conductive workpieces with controlled sparks. There is no contact and no cutting force between tool and part, so sharp internal corners, deep narrow rib slots, fine grooves and complex forms can be produced even in hardened steel.

At OSKA sinker EDM is in-house. We machine the electrode on our vertical machining centre and erode the mold under the same roof. The mold does not leave the workshop for a single operation, and responsibility for the dimensions stays in one place.

How sinker EDM works

The reverse of the required form is prepared as an electrode in copper or graphite. Electrode and workpiece are brought very close together in a dielectric fluid without touching. Thousands of sparks per second jump across the small gap; each one melts and removes a microscopic particle of steel, and the fluid flushes the particles away. As the electrode advances step by step, its form is reproduced in the steel.

Electrode (copper / graphite)Dielectric fluidWorkpiece (mold steel)Spark gapElectrode feed
The electrode never touches the steel; the sparks do the shaping.
  • Electrode design: the area to be eroded is separated from the 3D model and the electrode is modelled smaller by the spark gap.
  • Electrode manufacture: roughing and finishing electrodes are milled on the machining centre.
  • Set-up and alignment: electrode and mold part are positioned to the same reference.
  • Rough erosion: most of the material is removed at high energy.
  • Finish erosion: size and surface are brought to final values at low energy.
  • Inspection: depth and form are measured; the surface is prepared for polishing if needed.

Where we use it in a mold

Feature Why EDM?
Deep, thin rib slots A slender end mill deflects and breaks; an electrode reaches the same depth easily.
Sharp internal corners A round cutter leaves a radius; an electrode gives the corner the sharpness required.
Hardened mold parts Distortion from heat treatment is removed by eroding the final size afterwards.
Narrow deep pockets and fine grooves Areas with no tool access or poor chip evacuation.
Lettering, logos and date stamps Small raised or engraved details transfer cleanly from the electrode.
Matt (EDM) surface texture The even matt texture left by the sparks gives the molded part a blasted-like appearance.

Strengths and limits

Strengths

Independent of hardnessHardness does not affect machinability; the material only has to conduct.
No cutting forceThin walls and delicate areas are machined without deflection or burrs.
Forms beyond millingDeep, narrow and sharp-cornered geometry becomes possible.
Controlled surfaceThe energy setting selects anything from a coarse matt to a fine surface.

Limits

SlowerRemoval rate is lower than milling, so it is used only where needed.
Needs an electrodeEach form requires an electrode to be designed and machined, adding time and cost.
Conductive materials onlyPlastics and ceramics cannot be eroded.
Surface layerSparking leaves a thin recast layer; where a glossy surface is required it is removed by polishing.

Sinker EDM and wire EDM

Both work with sparks but do different jobs. In sinker EDM a shaped electrode plunges into the part and produces blind cavities. In wire EDM a thin wire cuts right through the part from one side to the other, so it only suits through profiles.

Sinker EDM Wire EDM
Tool Shaped copper or graphite electrode Continuously fed thin wire
Form produced Blind cavities, rib slots, 3D forms Through profiles, punch and die openings
Typical mold work Cavity details, sharp corners, lettering Insert pockets, ejector and core-pin profiles, cutting dies
At OSKA In-house Not available in-house

Frequently Asked Questions

Do you accept EDM-only work?

Yes. We consider erosion jobs independently of a mold project, with the electrode made by us or supplied by you.

Copper or graphite electrode?

Copper excels at fine surfaces and sharp detail; graphite at large, deep forms with fast removal and low electrode wear. We choose according to the size of the form and the surface required.

What does an EDM surface look like on the part?

The spark texture transfers to the part as an even matt surface. For a glossy part the cavity is polished after erosion.

What do you need from us?

The 3D model, the areas to be eroded, the material and hardness, and the surface quality required.

Request a Quote

Kalıp ve hassas parça işleriniz için üretim ortağınız

Kokil, plastik enjeksiyon ve alüminyum enjeksiyon kalıpları ile CNC talaşlı imalat tek atölyede. Teknik resminizi gönderin, birlikte değerlendirelim.

Bize Ulaşın
Kasım 16, 2026

Stainless Steel Grades in CNC Machining: 303, 304, 316, 420 and 17-4 PH

Devamını oku
Kasım 16, 2026

CNC İşlemede Paslanmaz Çelik Türleri: 303, 304, 316, 420 ve 17-4 PH

Devamını oku
Tüm haberler ve yazılar