The surface of a part decides more than its appearance: wear, corrosion, friction, sealing and, in a mold, how the part releases. This guide summarises the surface and finishing processes most often used on machined parts and molds, the materials they suit, and how to call them out on a drawing.
As machinedMechanical finishesCoatingsHeat treatmentMold cavity finishesHow to chooseOn the drawingFAQ
As-machined surface
The fastest and most economical option. The part is delivered as it leaves the machine: tool marks are visible, sharp edges are broken and burrs removed. In standard machining the roughness is typically around Ra 3.2 µm; finishing passes can reach Ra 1.6 and 0.8 µm, but each step adds machining time. Hidden surfaces with no fit function need nothing more.
Mechanical finishes
| Process | What it gives | Suitable materials | Watch out for |
|---|---|---|---|
| Bead / grit blasting | Even matt surface that hides tool marks; preparation for paint and coating | Steel, stainless, aluminium | Slightly affects size; mask precise fit surfaces |
| Vibratory finishing | Bulk deburring and edge rounding of small parts | Most metals | Not for edges that must stay sharp |
| Brushing | Directional decorative grain | Stainless, aluminium | State the grain direction on visible faces |
| Grinding | Tight tolerance and low roughness; final size on hardened surfaces | Steels | Leave grinding stock |
| Polishing | Bright, low-roughness surface | Steel, stainless, aluminium, brass | Labour-intensive; request only where needed |
Coatings and conversion processes
| Process | What it gives | Suitable materials | Watch out for |
|---|---|---|---|
| Anodising | Corrosion and scratch resistance, colour, electrical insulation | Aluminium | The layer changes dimensions; threads and precise holes can be masked |
| Hard anodising | Thicker, harder layer for wear resistance | Aluminium | Limited colours; allow for the layer |
| Powder coating | Thick, impact-resistant coloured coating | Steel, aluminium | Thick layer affects fits; part must withstand oven temperature |
| Zinc plating | Economical corrosion protection for steel | Steel | Assess hydrogen embrittlement risk on high-strength steels |
| Nickel and hard chrome plating | Wear and corrosion resistance, low friction | Steel, copper alloys | Include plating thickness in the tolerance |
| Black oxide | Dark surface with almost no dimensional change, light protection | Steel | Not sufficient outdoors on its own; used oiled |
| Passivation | Strengthens the natural protective layer of stainless steel | Stainless steel | Does not change appearance or size |
Heat treatment and surface hardening
Heat treatment is not a cosmetic process, but it changes surface behaviour more than anything else. Sequence matters: because hardening can cause distortion, precise dimensions are usually produced after heat treatment by grinding, hard milling or sinker EDM.
| Process | What it gives | Typical use |
|---|---|---|
| Quench and temper | Balance of strength and toughness through the section | Shafts, fasteners, mold inserts |
| Through hardening | High hardness and wear resistance | Mold cores, cutting and wear parts |
| Case hardening | Hard surface, tough core | Gears, pins, impact-loaded parts |
| Nitriding | Hard, low-friction surface with little distortion; resists soldering | Ejectors, core pins, die-casting and gravity die surfaces |
| Stress relieving | Reduces machining and welding stresses, stabilises dimensions | Large plates, welded frames, rough-machined mold parts |
Mold cavity finishes
In plastic injection the part surface is a copy of the cavity surface, so the gloss or texture wanted on the part is applied to the mold steel.
| Cavity finish | Appearance on the part | Note |
|---|---|---|
| As machined | Light tool marks, non-visible faces | Most economical; adequate for internal and technical faces |
| Stoned / papered (semi-gloss) | Even, mark-free but not glossy | Standard choice for most technical parts |
| Mirror polish | High gloss, clarity on transparent parts | Requires a clean steel suited to polishing |
| EDM (matt) texture | Even matt surface | Natural texture of sinker EDM; increase draft in textured areas |
| Blasted | Fine matt surface | Makes the surface uniform and hides small marks |
| Chemical texturing | Leather, wood-grain, geometric patterns | Extra draft needed according to texture depth |
Textured and matt surfaces make ejection harder. The deeper the texture, the more draft is needed; with too little draft the part shows scuffing and stress whitening.
Which finish should I choose?
| Need | Suggestion |
|---|---|
| Corrosion and scratch resistance on aluminium | Anodising; hard anodising if wear is also involved |
| Economical rust protection on steel | Zinc plating; black oxide and oil where size must not change |
| Uniform matt look that hides tool marks | Blasting; followed by anodising on aluminium |
| Coloured, impact-resistant outer surface | Powder coating |
| Wear resistance on sliding surfaces | Nitriding or hard chrome; hard anodising on aluminium |
| Tight-tolerance fit surface | Grinding; allow for the layer if coating follows |
| Glossy plastic part | Mirror-polished cavity in a suitable steel |
How to specify it on the drawing
- State roughness as Ra or Rz, and only on the surfaces that need it; a tight value on the whole part raises cost for nothing.
- For coatings give the process, thickness and colour, and say whether dimensions apply before or after coating.
- Mark surfaces that must not be coated or blasted: threads, fit diameters, contact faces.
- For heat treatment give the target hardness and, where needed, the case depth.
- Mark visible surfaces separately so racking and clamping marks are kept away from them.
Frequently Asked Questions
Does coating change the size of the part?
Yes, most coatings add a layer. In anodising part of the layer grows into the surface and part outwards. On precise fits the allowance is built into the machined size, or the surface is masked.
Is a low roughness on every surface better?
No. Low roughness means extra passes, grinding or polishing. Ask for it only where sealing, bearing or appearance requires it.
Which processes are done in your workshop?
Machining, EDM, bench fitting and polishing are done in-house. For processes that need dedicated plants, such as plating and heat treatment, simply tell us your requirement at the quotation stage and the machining sequence is planned around it.
Which materials can be anodised?
Anodising is specific to aluminium. On steel, zinc or nickel plating or black oxide give comparable protection.